Index Properties |
Test Method |
Unit |
MD Values |
TD Values |
Polymer |
- |
- |
PP |
- |
Tensile Strength @ 2% Strain |
ASTM D 6637 |
kN/m |
7 |
7 |
Tensile Strength @ 5% Strain |
ASTM D 6637 |
kN/m |
14 |
14 |
Ultimate Tensile Strength |
ASTM D 6637 |
kN/m |
20 |
20 |
|
Structural Integrity |
|
|
|
|
Junction Efficiency |
GRI GG2 |
% |
90 |
- |
|
Flame Retardant Properties |
|
Maximum Flame Propagation |
ASTP 5011 |
m |
1.2 |
Average Duration of Burning for Test Set |
ASTP 5011 |
minute |
1.0(max) |
Maximum Duration of Burning for Single Test |
ASTP 5011 |
minute |
2.0 |
|
Dimensions |
|
Aperture Dimensions |
|
mm |
60 |
65 |
Roll Width |
|
m |
1.85/ 3.70 |
Roll Length |
|
m |
50 |